Moisture Meter Manuals & Species Adjustment Tables
Questions? Need help with specific gravity settings? Give us a call: (541) 291-5124
Wood Species Settings Database – 7500+ Species Listed
Species Settings for Common Flooring Products
Immersion Method to determine wood SG (use if you can’t find your species above)
Bamboo Flooring Settings for Wagner Meters Handheld Moisture Meters
Download Species Settings Table
Specific Gravity Summary
The specific gravity (density) values for a species* are based on the best, current world data, and are used to determine the correct species settings factor within the meter. The values are average density values for the species. A coefficient of variation (COV) of about 10% describes the variability inherent in many common domestic (US) species.
* The specific gravity based on oven dry weight and 12% moisture content.