Cedar Woods Remarkable Weather Resistance
When choosing wood for an outdoor project, durability matters most. You want a material that can withstand weather, resist decay, and hold its appearance for years.
That’s where cedar stands out.
From gazebos and fences to saunas and outdoor furniture, cedar has earned its reputation for longevity. But what makes it perform the way it does in exposed conditions?
In this guide, we’ll cover:
Whether you’re a contractor, woodworker, or DIY enthusiast, understanding how cedar interacts with the environment will help you get more out of it. And if you want your cedar projects to last, start by measuring the moisture content before installation.
Cedar’s Origin
Western Red Cedar and Northern White Cedar are coniferous members of the Cypress family Cupressaceae. The Western Red Cedar tree, or Thuja plicata, primarily grows in the Pacific Northwest region of the US.
The Northern White Cedar tree, or Thuja occidentalis, primarily grows in Eastern-Southeastern Canada and adjacent states of New England and the Great Lakes region west to Minnesota.
Western Red Cedar is a large-to-very-large tree and can grow in some areas up to 230 ft. tall. It is also long-lived and some trees can live well over a thousand years, with the oldest verified being 1,460 years old.
By contrast, Northern White cedar is a smaller tree and commonly grows up to 50 ft. tall, but a few trees can grow as large as 80 ft. It grows relatively slowly in swamp areas or on other saturated lowland sites and some trees can reach the ages of 400 years and greater in these habitats. One tree from Ontario was dated at more than 1,650 years old.
Both species produce the distinct “cedar” scent. This is caused by the oils and acids produced by both wood species. These are known scientifically as “polyoxyphenols” which give cedar its distinctive and pleasant aroma. The phenols are also responsible for cedar’s natural resistance to moisture, decay and insect infestation.
The natural resistance provided by the oils and acids is what makes these species more popular in outdoor applications. Properly finished, cedar can last for decades even in harsh environments.
Properties of Cedar Wood
Western Red Cedar heartwood is known for its durability, as it has a natural resistance to moisture, decay and insect damage. According to the Western Red Cedar Lumber Association, it has twice the stability of most commonly available softwoods, a result of its low density and shrinkage factors. It produces long, lightweight lengths of timber with a fine straight grain and uniform texture.
This makes it easy to cut, saw and nail with common tools. It also can be planed to a smooth surface or machined to any pattern. It can hold glue bonds and also provides a good base for many types of paints and stains since it lacks pitch and resin.
It is also valued for its distinct aroma that is commonly believed to discourage moth and carpet beetle larvae infestations. All of these factors make it a popular choice for both interior and exterior home use.
Free Download – 4 Reasons Your Hardwood Flooring Failed
Northern White Cedar is the lightest commercial domestic wood in the United States. It is even-grained and finely textured. The heartwood is resistant to decay and subterranean termites. It is easy to work, glues well and holds paint well.
It also experiences little dimensional change, but it should be noted that the wood is soft and has low mechanical properties such as bending strength and nail-holding abilities. The wood has been primarily used to make rustic fencing and posts, but can also be used for cabin logs, lumber, poles, shingles, and other specialty type products.
Woodworking with Cedar
If you’re thinking about starting a project with cedar, you may need to know the moisture content of the wood before beginning.
Cedar’s natural longevity can be drastically shortened if it is not taken care of. If you want to get the longest life out of your cedar project, consider basic moisture content (MC) measurement and management. All wood species, even cedar, are subject to natural processes. Moisture resides in the cell walls and cell cavities of all wood.
Once a tree is cut and kiln-dried, its MC still fluctuates according to changes in the relative humidity (RH) and temperature of its surrounding environment. This is especially pertinent to cedar users because so many use the wood outdoors.
Wagner Meters produces several moisture meters for wood, depending on the application. The Orion® 930 Dual Depth Pinless Wood Moisture Meter is the replacement for the MMC220 legacy meter.
The Orion 930 measures the MC in common softwoods (such as cedar), hardwoods and also exotic wood species at two different depth settings. Even do-it-yourself wood flooring restorers could utilize the Orion 920 shallow depth meter to determine when the wood flooring surface has acclimated properly.
Do your part to protect the longevity of your cedar. Measure its MC before leaving it to the elements.
Troy Edwards is Technical Service Supervisor for Wagner Meters, Inc., where he oversees manufacturing, quality control and IT service for their electronic measurement products for the building and construction industry. Troy holds an AAS in Electronics Technology and has over 20 years’ experience in various electronic manufacturing and production positions.
Last updated on October 23rd, 2026
Hi,
Is it safe to use 1X6 red western cedar for pool coping, it will go over aluminum trim of the pool. I plan to paint it Stoneffects for creating a non-slip surface.
Hi-
How does WRC compare to redwood for decay resistance? I know the grading standards change but I’m only considering lumber with no sapwood involvement. Are they similar in strength? I’m doing a small project in the Sierra Foothills and prolonged extreme temperature exposure is common here, both high and low temperatures.
Thanks-
I am going to be using northern cedar (grown her in Michigan) for dock posts in a freshwater lake. The trees still have their bark on them which I will remove before water jetting them 5-7 feet into the lake bottom. Should they be sealed first? From what I have read, it seems as though the buried end (at least) should be sealed. Thanks, Bob
Bob,
I would agree to seal the bottom first.
I am doing a research paper on the Cedars of Lebanon. In your writing, you mention how the polyoxyphenols, the acids and oils, help prevent rot and prevent the infestation of bugs(at least the destruction of the wood due to bugs). What do the polyoxyphenols actually do to help protect humidity and insects?
-Ford
It’s really interesting how a variety of cedarwood is naturally resistant to moisture, decay, and insect damage. I’ve seen an ornamental cedar fence on my way home and immediately considered it as an option for fencing material. Since we live in a town where we experience harsh weather conditions, I think its best to choose cedar. I’d consult fence contractors to see how soon we can hire their services and have this installed.
What would you recommend and expect cedar slats longevity for gate slats in the Phoenix AZ climate? Is any treatment recommended for this application?
John
John, I would recommend a treatment that will slow down any additional drying that may occur in a drier climate. Additionally, here is a link to a document that should give you some good information:
https://www.uslumber.com/MainSite/Store1/Content/SiteContent/1/home/docs/cedar_Brochure.pdf
Before treating, make sure to use an accurate moisture meter to check the moisture content of the cedar slats.
Wow, it’s amazing to know that cedar is resistant to both decay and termites. I was initially only looking for a water-resistant material for a roofing job but I never knew cedar is more than just that. I will definitely replace my current asphalt shingles with cedar.
What was done with the tree found dated so old in Ontario?
Hi John,
We don’t have any information on the tree. We just know that there was documentation that one of the oldest ones as old as 1,650 years. https://plants.usda.gov/plantguide/pdf/cs_thoc2.pdf
Hi,
My name is Michael and I am the sustainability coordinator for the University of Washington. We are currently building a computer operated solar kiln and we have some questions. We would like to set it to a standard temperature and humidity and were wondering if you had any recommendations?
Thanks!
Michael
Hi Michael,
I suggest that you contact the Oregon State University Forest Products Department if your own Forest Products department cannot provide some guidance.
Thanks,
Ron