How Moisture Affects Your Flooring’s Durability and Performance

Whether it’s hardwood flooring in a family home, concrete flooring in a school gym, or brand new tile at a local restaurant, flooring sets the tone and functionality of any space. These floors should work for you and last a long time.

That all changes, though, if moisture is left unchecked and uncontrolled.

The good news is that moisture problems can be prevented. At Wagner Meters, we make tools that help you catch moisture issues before they become flooring problems, so your floors, and your clients’ floors, look great and last.

Keep reading to learn how detrimental moisture can be to your floors.

Specifically, this article will cover:

Let’s start by understanding the building blocks of moisture issues.

Why Moisture Matters and Why You Should Care

Moisture is pretty much everywhere: in the air, in the ground, inside, outside, and, yes, even in your flooring.

The problem is not the presence of moisture; it’s the presence of too much moisture.

This moisture, when left unmanaged, can be detrimental to flooring. It can cause materials to break down and, depending on the material, can cause severe warping, mold growth, and dangerous structural damage.

Some materials, like wood, are hygroscopic, meaning they absorb or release moisture depending on their environment. If the ambient conditions are too wet, the wood won’t be able to release moisture. If, on the other hand, the conditions are too dry and the wood itself is overdried, the wood may shrink, split, or become brittle.

Other materials, like concrete, can stay wet for a long time if they’re covered before the moisture in the mix has a chance to evaporate.

Whatever flooring you’re using, unmanaged moisture is likely to cause problems.

Let’s break down the impact of moisture on specific flooring to see how important moisture management is.

Worn oak strip floor with uneven, separated boards

Buckling, cupping, crowning, and other types of warping will make even the prettiest wood floor look bad.

How Does Moisture Impact Wood Flooring?

If wood flooring takes on moisture, it expands. If it releases moisture, it shrinks. That’s because, as mentioned earlier, wood is hygroscopic: it acts like a sponge in response to its environment.

So when wood flooring is put down and its moisture content (MC) doesn’t match the equilibrium moisture content (EMC) of the installation location, you’re asking for trouble.

Warping can take many forms. It can happen if the wood is too wet or too dry, or if the subfloor beneath it hasn’t been properly dried.

Warping can look like:

  • Bow: the plank curves along its length, from end to end
  • Crook: the edge of the plank curves from end to end
  • Cupping: the edges of a plank are higher than its center, in a U shape
  • Crowning: the opposite of cupping. The center of the plank is higher than the edges.
  • Twist: the corners of a plank are no longer in the same plane

Even without warping, the normal seasonal shrinking and swelling of wood can cause cupping or unsightly gaps if it isn’t accounted for during installation.

So, if your wood floors come from a low-humidity environment but end up in a high-humidity environment, they will expand, which could cause cupping or buckling.

How Does Moisture Impact Concrete Flooring?

A slab that’s too wet can lead to mold growth in the flooring and adhesives above it, which is both unsightly and a health concern. Wet concrete also harms any flooring installed on top of it.

Moisture from a concrete subfloor can migrate through the slab and into the flooring above it, whether that be wood, laminate, or tile. This kind of moisture can cause warping, breakdown of adhesives, or cracking.

Water is an essential part of the concrete mix. Even after the concrete has hardened and looks dry, it can still hold moisture deep below the surface.

This moisture can take a long time to evaporate, so it takes a while for concrete to be truly dry. If the concrete isn’t given the time and conditions it needs to dry, the consequences can be serious.

How Does Moisture Impact Tile Flooring?

At first glance, tile would seem to be unaffected by moisture. After all, it’s commonly used in humid places like bathrooms, kitchens, and basements. But while it’s true that tile is more resistant to moisture than wood flooring, it’s not invincible.

Most of the moisture that affects tile comes from the subfloor. Moisture constantly coming up from a wet subfloor can break down grout and setting materials, loosen or crack tiles, and eventually allow mold and mildew to grow beneath them.

In the end, almost no flooring is immune to unmanaged moisture. So how can you tell whether moisture is affecting your floor? Here’s how to spot the early signs, and the real solution: prevention.

Spotting the Early Signs of Moisture Damage

Moisture damage is one of those things that happens slowly, and if you catch it soon enough, you can solve the problem with little to no consequences. That being said, moisture can also go undetected for a long time. With enough time, it can cause irreversible damage to flooring.

But if you know the signs, you can catch the damage early. Here are some signs to look out for:

  • Warping, like cupping, crowning, or twisting
  • Buckling
  • Discoloration
  • Musty smells
  • Loose tiles or squeaky boards

No matter how good you get at spying out these early signs, the best solution is to prevent the problem in the first place. That’s where we come in.

Here are the products that make preventing and monitoring moisture damage easier.

Hand holding an Orion 950 pinless moisture meter flat on a wood flooring board

The Orion® 950 is easy to use for anyone who works with wood.

Protect Your Flooring with Wagner Meters

We have several products to help you manage and monitor moisture. Here are three that can save you time, money, and headaches.

Orion Pinless Wood Moisture Meters

Our Orion® line of pinless meters helps your hardwood floors last longer and stay beautiful.

A high-quality pinless moisture meter, like the Orion 950, will tell you the moisture content (MC) of a plank of wood quickly, accurately, and without any pinhole damage.

When you measure the MC of several planks, you’ll know whether it’s close to the EMC for the installation location, which helps keep the planks from warping or buckling.

And, if you take your moisture meter with you when you purchase wood, you’ll be able to measure MC prior to purchase, meaning you won’t buy wood that needs time and money to dry out.

Illustration of a DataGrabber with Bluetooth installed in a concrete slab

The DataGrabber® makes concrete moisture monitoring nearly effortless.

Rapid RH® System

In-situ relative humidity testing, with sensors placed inside the slab, is widely considered the most reliable way to determine the moisture condition of a concrete slab. That’s where our Rapid RH system comes in.

It’s easy hands-on monitoring that involves drilling small holes into the concrete slab and inserting sensors. These sensors, our Rapid RH L6 Smart Sensors, give you the data you need to make informed decisions about the slab.

And if you want to take this system from hands-on monitoring to automatic on-site monitoring, all you have to do is attach the DataGrabber with Bluetooth® to the in-slab sensor.

Then, instead of reading each sensor yourself, you can automatically upload the stored readings to your smartphone with the free DataMaster L6 app when you return to the site.

Floor Sentry®

If you want to make your floor a smart floor, Floor Sentry is the ticket. This card-sized data logger is embedded in the wood floor.

Once it’s installed, pair it with the Wagner Sentry app to monitor temperature and relative humidity in the floor for years (its battery can last up to 8 years, depending on settings). You can also set alarms for when humidity or temperature goes outside a set range.
Learn about Floor Sentry, the embedded wood floor data logger
When you monitor ambient conditions, you’re not just getting data. You’re empowering your clients with the knowledge they need to maintain the beauty and longevity of their floors.

The Moral of the Story? Manage Moisture Proactively!

If you take one thing from this article, let it be this: moisture must be managed. Otherwise, you and the floors you install could be in big trouble.

The products above make it much easier to manage moisture and prevent moisture damage.