RH Testing: Why Drill at 40% Depth

Jason Spangler, Vice President of Sales for Wagner Meters, explains the science behind the 40% depth requirement in ASTM F2170, the depth at which a slab drying from one side shows the moisture condition it will reach once a floor covering is down.