In a new partnership between Rapid RH® L6 by Wagner Meters and CLīMIT™, we introduce you to the True Remote Monitoring™ System.
With True Remote Monitoring, you can view real-time jobsite conditions from anywhere in the world—so long as you have cellular network connectivity. This system combines the best of Rapid RH moisture measurement technology with the latest software, hardware and cloud connectivity technology from CLīMIT.
It is designed to protect your installation and reputation, while improving the profitability of your company.
TO GET YOUR HARDWARE
Relative humidity (RH) testing, standardized as ASTM F2170, involves placing in situ RH sensors at specific depths in the slab.
After allowing the RH sensors to equilibrate, measurements of RH and temperature are taken to assess the overall moisture condition of the slab.
The DataGrabber with Bluetooth engages the L6 Smart Sensor to collect and store concrete RH and temperature readings within the sensor according to a set time interval.
This information is then transmitted via Bluetooth signal and the Rapid RH® L6 DataGrabber® Range Extender (DGRE) to the CLīMIT sensor.
CLīMIT sensors work with the Rapid RH sensor and DataGrabber with Bluetooth to monitor jobsite ambient climate conditions, concrete relative humidity, and temperature hourly, 24/7/365.
All data is transmitted to a cloud database via the cellular network for comparison against manufacturer’s specifications.
If site conditions are out of range, project leads immediately get alerts on their phone so corrective actions can be taken quickly before issues escalate.
Protect your installation and reputation, while improving the profitability of your company.
All you need to add to your toolbox is:
With this integrated system, contractors and flooring installation professionals can save time and money and maximize productivity by remotely monitoring their jobsites in real time, 24/7/365 days a year.
Return to the jobsite only when the concrete subfloor is ready for the next phase.
| Cookie | Duration | Description |
|---|---|---|
| cookielawinfo-checkbox-analytics | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Analytics". |
| cookielawinfo-checkbox-functional | 11 months | The cookie is set by GDPR cookie consent to record the user consent for the cookies in the category "Functional". |
| cookielawinfo-checkbox-necessary | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookies is used to store the user consent for the cookies in the category "Necessary". |
| cookielawinfo-checkbox-others | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Other. |
| cookielawinfo-checkbox-performance | 11 months | This cookie is set by GDPR Cookie Consent plugin. The cookie is used to store the user consent for the cookies in the category "Performance". |
| viewed_cookie_policy | 11 months | The cookie is set by the GDPR Cookie Consent plugin and is used to store whether or not user has consented to the use of cookies. It does not store any personal data. |