C575 Analog Concrete Moisture Meter

This product is no longer available. We suggest the Rapid RH 4.0 Complete Starter Kit instead.

About the C575 Analog Concrete Moisture Meter


SKU: 890-57501-001

NOTE: Handheld meters used at the surface can only be used to determine what locations to place other tests.

This product is no longer available. We suggest the Rapid RH® 4.0 Complete Starter Kit instead.

The C575 Concrete Moisture Meter provides relative readings on concrete slabs and is used as a qualitative quick scan test to determine the most appropriate areas to place true quantitative tests. For ASTM standard quantitative tests, visit our Rapid RH® site

Materials to Measure

Concrete Similar Densities

Specific Applications

There is no correlation between moisture content (MC) % of the concrete and the readings with concrete moisture meters.

The MC % is not an exact percentage and should not be used to determine the moisture in concrete. The readings are relative readings and should only be used to determine if further testing is needed and where to place further tests such as the Rapid RH®. The C575 meter gives a general moisture indication to 3/4″.

Always check with the flooring manufacturer for further testing and warranty requirements.

Meter Specifications

Size & Weight: Length – 4 9/16″ Width – 2 3/4″ Height – 1 9/16″
Power: 9-volt battery (included); Auto Power Shut Down – 60 seconds
Depth of Measurement: 3/4″
Measurement Scale: 0 – 20 Analog Display
Scanning Area: 1 1/2″ x 2 1/2″
Calibration: Calibration block not necessary – can be verified without the calibration block
Other: 
1-Year Warranty
Hard Plastic Case Included
Teflon® Pad Protects Sensor Plate from Abrasive Surfaces