How do pin-type moisture meters work?

Pin-type moisture meters work on a primitive, resistance principle that basically measures the flow of electricity through a substance.

This method is subject to many environmental variables that can dramatically affect readings such as chemicals in the water trapped within the wood and the temperature of the wood.

The following two tabs change content below.
Wagner Meters is a family-owned American business that aims to provide solutions in moisture measurement technology that will enhance the quality and value of each customer's project. With an almost 60-year legacy of innovation, Wagner continues to be a resource for both individual craftsmen and high-performance commercial endeavors.