Can anyone tell me what is the technical / scientific significance of the "moisture content" (see left hand side in pink under the rH % measurements) http://www.concreteconstruction.net/concrete-articles/how-heavy-is-concrete.aspx

Are they saying that is the moisture content via the gravimetric method? http://www.cement.org/tech/faq_air_tests.asp


Following article shows the 'moisture content' but not in %.
http://www.cement.org/tech/faq_moisture_content.asp ?

Perhaps someone can explain this, I bookmarked the 1st article to try to figure out but I'm afraid I'm no engineer or PhD.








Messages In This Thread
Moisture Content - eaadams - 02-26-2011, 10:58 AM
RE: Moisture Content - Ernesto - 02-26-2011, 03:04 PM
RE: Moisture Content - CC Solutions - 02-26-2011, 05:16 PM
RE: Moisture Content - iris54ford - 02-28-2011, 01:43 AM
RE: Moisture Content - Ernesto - 02-28-2011, 08:26 AM
RE: Moisture Content - CC Solutions - 02-28-2011, 11:08 AM
RE: Moisture Content - Ernesto - 02-28-2011, 05:01 PM
RE: Moisture Content - CC Solutions - 02-28-2011, 05:35 PM
RE: Moisture Content - DeanC - 03-03-2011, 10:18 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,629 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 28,327 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,361 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 10,112 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 15,209 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 73,988 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 17,160 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 25,555 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 49,930 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM

Users browsing this thread:
1 Guest(s)