#Login Register
RH and Temperature Question
  • 0 Vote(s) - 0 Average


09-30-2008, 08:01 AM #1
Chris Reynold Newbie *
Status: Offline Posts:2 Threads:2 Joined:Sep 2008
I drilled several test holes, inserted sleeves and returned to the first test hole about 15-20 minutes later. Inserted a RapidRH reader in the first test hole and got a temp. of 85 and a RH of 75. The other test holes were in this same general range. Later in the day I took readings and the temp was down around 70 and the RH was up around 80. Can anyone help me understand what is going on?








Messages In This Thread
RH and Temperature Question - Chris Reynold - 09-30-2008, 08:01 AM
RE: RH and Temperature Question - rthompson - 10-01-2008, 03:39 PM
RE: RH and Temperature Question - Hbenavente - 10-03-2008, 02:09 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 3,475 Views
Last Post by rapidrhrep
05-07-2015, 04:18 PM