(02-26-2011, 12:10 AM)barry88rowe Wrote:  I have no idea why the pH in your influent water varies, I'd check environmental factors such as rainfall, temperature, and time of year for correlation.

Welcome Barry!!

Most of the concrete slabs we deal with will be either on grade with a vapor retarder below them or raised and poured in a pan. There should really be no influent moisture, only the original moisture included in the concrete mix. Temperature should be at service conditions.

Actually if you have incoming water, the PH is irrelevant! You have a real problem. Big Grin

If I'm off-base please don't be shy to say so! I get that a lot around here. Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 11,222 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,191 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 39,867 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 100,739 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,439 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 91,994 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 5,817 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 73,742 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 105,784 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 41,479 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM

Users browsing this thread:
1 Guest(s)