(02-26-2011, 12:10 AM)barry88rowe Wrote:  I have no idea why the pH in your influent water varies, I'd check environmental factors such as rainfall, temperature, and time of year for correlation.

Welcome Barry!!

Most of the concrete slabs we deal with will be either on grade with a vapor retarder below them or raised and poured in a pan. There should really be no influent moisture, only the original moisture included in the concrete mix. Temperature should be at service conditions.

Actually if you have incoming water, the PH is irrelevant! You have a real problem. Big Grin

If I'm off-base please don't be shy to say so! I get that a lot around here. Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 14,321 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 37,136 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 44,864 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 116,450 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 17,226 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 105,132 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 6,740 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 84,018 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 122,472 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 47,146 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM

Users browsing this thread:
1 Guest(s)