And there are more than just EI meters. (electrical impedance) The GE meeter is not EI I don't think. I think it is some sort of RF as it doesn't have electrical contacts.

But every tester I've ever used uses EI to find the high points in a slab to set his probes (or set a higher concentration of probes in that area).








Messages In This Thread
Concrete Moisture Meter - DeanC - 02-04-2011, 09:34 AM
RE: Concrete Moisture Meter - CC Solutions - 02-05-2011, 09:37 AM
RE: Concrete Moisture Meter - DeanC - 02-05-2011, 07:22 PM
RE: Concrete Moisture Meter - CC Solutions - 02-06-2011, 11:26 AM
RE: Concrete Moisture Meter - DeanC - 02-07-2011, 10:30 AM
RE: Concrete Moisture Meter - CC Solutions - 02-07-2011, 11:10 AM
RE: Concrete Moisture Meter - eaadams - 02-09-2011, 10:36 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,615 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 11,245 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,248 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,351 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
9 Replies 39,903 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 10,094 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 101,003 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,475 Views
Last Post by eaadams
01-30-2013, 04:43 PM
4 Replies 15,165 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
32 Replies 92,197 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM

Users browsing this thread:
1 Guest(s)