#Login Register
RH and MVER Concrete Moisture Conversion table
  • 0 Vote(s) - 0 Average


02-05-2011, 10:08 AM #3
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
There is NO CORRELATION between RH and MVER.

Think of it this way:

You have a dry slab, 50 years old, suspended, RH is 55%.
You wet that slab for 24 hours, flood it.
The slab RH is still 55%, the surface water soaked in 1/4" to 1/2" or so.
A CaCl test will read about 12lbs placed on that wet surface.

Conversely a slab in a very dry building laying on a wet subsoil can read 3lbs MVER because the surface is very dry, but the lower portion of the slab is very wet. RH readings can easily reach 90%+. Cover that slab with a moisture sensitive flooring and the concrete will continue to absorb water and RH will climb even higher.

I have personally seen these scenarios, they are very real.


JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
RH and MVER Concrete Moisture Conversion table - jpeters - 01-28-2011, 03:49 PM
RE: RH and MVER Concrete Moisture Conversion table - eaadams - 02-03-2011, 12:10 PM
RE: RH and MVER Concrete Moisture Conversion table - CC Solutions - 02-05-2011, 10:08 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,972 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 14,416 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 37,418 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 9,197 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
9 Replies 45,039 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 12,080 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 116,966 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 17,300 Views
Last Post by eaadams
01-30-2013, 04:43 PM
4 Replies 17,906 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM

Users browsing this thread:
1 Guest(s)