I found this conversion chart on a blog and wondered if anyone else had seen this and if it's accurate?

"<75% would be equivalent to <3 lbs/sf
76%-85% would be equivalent to 3-6 lbs/sf
86%-90% would be equivalent to 6-12lbs/sf
>91% we are going to want to look very closely at the floor before moving forward"

I found it at this blog: http://www.florock.net/blog/2010/06/09/concrete-floor-coating-2010








Messages In This Thread
RH and MVER Concrete Moisture Conversion table - jpeters - 01-28-2011, 03:49 PM
RE: RH and MVER Concrete Moisture Conversion table - eaadams - 02-03-2011, 12:10 PM
RE: RH and MVER Concrete Moisture Conversion table - CC Solutions - 02-05-2011, 10:08 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,630 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 13,957 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 35,948 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 8,948 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
9 Replies 44,211 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 11,787 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 114,558 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 16,887 Views
Last Post by eaadams
01-30-2013, 04:43 PM
4 Replies 17,518 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM

Users browsing this thread:
1 Guest(s)