11-11-2010, 02:10 PM #1
GregR Newbie *
Status: Offline Posts:6 Threads:2 Joined:Nov 2010
I recently read a probe (New Wagner Orange Reader) and got a reading of 89% at 69°. I immediately read the test again and got a reading of 86% at 71°. I read it a third time at 83% at 72°.

Can I assume the first reading is correct? My assumption is when taking multiple readings the electrical current running thru the sensor is causing it to heat up and reducing the RH in the hole. Is this correct?








Messages In This Thread
Multiple Readings? - GregR - 11-11-2010, 02:10 PM
RE: Multiple Readings? - CC Solutions - 11-13-2010, 11:34 AM
RE: Multiple Readings? - Ernesto - 11-14-2010, 10:18 AM
RE: Multiple Readings? - GregR - 11-14-2010, 11:31 AM
RE: Multiple Readings? - RSmith - 11-15-2010, 10:57 AM
RE: Multiple Readings? - GregR - 11-16-2010, 08:08 AM
RE: Multiple Readings? - CC Solutions - 11-19-2010, 05:26 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
49 Replies 126,914 Views
Last Post by Ernesto
12-08-2011, 06:03 PM
1 Replies 10,798 Views
Last Post by rthompson
10-15-2008, 11:00 AM

Users browsing this thread:
1 Guest(s)