  • 0 Vote(s) - 0 Average


12-11-2010, 06:11 PM #31
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(12-10-2010, 11:09 PM)Selah4Makens Wrote:  The Concrete Encounter is a hand-held electronic moisture meter that utilizes non-destructive impedance measurement for moisture determination. Parallel co-planer electrodes are mounted on the unit's base which transmit low-frequency signals into the concrete... The results give the average moisture content to a depth of 2-6 inches during the drying period.

I will argue that 2-6 inches all day long! EI readings are as much witchcraft and hocus-pocus as diving rods and crystal balls.... In my humble opinion that is... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 9,762 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 32,334 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 8,250 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 11,034 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 16,484 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 78,597 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 18,306 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 27,338 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 53,075 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM

Users browsing this thread:
1 Guest(s)