I have a job not to far off from starting that does not have HVAC on yet. I have put down some probes just to keep an eye on the %. At his time with the temp around 72 and the humidity around 54% the probes read between low70% and high 70%. I know that the HVAC has to be running for the test to pass ASTM, but at the Wagner RH webinar (starnet) they made it sound like you should be able to tell if the concrete is in a drying mode. With that being said what is your thoughts? Is the % they are at now a good sign or will they jump up when the HVAC goes on?
What is your thoughts?
Bob Huesgen, Zickel Flooring St louis mo

09-28-2010, 10:08 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
The temperature of the slab is what?

If the slab is on grade, the temperature will stay around the upper 60's always. The readings you are getting will stay about the same.

Is this a new slab with a good vapor retarder placed in contact with the bottom of the slab? If so it sounds like you have a pretty darn nice slab there.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

09-30-2010, 08:27 AM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
How old is that slab? Enclosed?

It has been my experience that HVAC affects CaCl more than rH.








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,328 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 10,775 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 85,452 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 143,831 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 16,128 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 56,787 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
36 Replies 105,057 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 31,836 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM
11 Replies 39,092 Views
Last Post by CC Solutions
09-20-2010, 03:01 PM
15 Replies 48,539 Views
Last Post by Ernesto
01-12-2010, 10:56 AM

Users browsing this thread:
1 Guest(s)