(09-20-2010, 02:26 PM)CC Solutions Wrote:  PH and moisture will go hand in hand also.

I disagree. I have seen moisture results well below failure, low 80's%, but pH be in the 12 range (newer slabs). I have seen low pH and high moisture (old slabs).