F710 states that the slab should be tested for ph but i don't see a number of tests per sf. how many areas have to be tested and were is it stated.








Messages In This Thread
PH TESTING - MINUS - 09-02-2010, 10:04 AM
RE: PH TESTING - Ernesto - 09-03-2010, 08:11 AM
RE: PH TESTING - CC Solutions - 09-20-2010, 02:26 PM
RE: PH TESTING - hausenheimer - 07-22-2013, 07:07 AM
RE: PH TESTING - CC Solutions - 07-22-2013, 08:47 AM
RE: PH TESTING - hersitervery - 04-02-2014, 04:10 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
32 Replies 81,810 Views
Last Post by hausenheimer
03-28-2013, 08:45 AM