Well, I guess I just ask! I check the prints, look for cored holes, cut-outs at HVAC shafts, whatever, but I need to rely on the owner or General's knowledge of how thick the slab is.

That said, there is always risk that the slab isn't what they think it is! Multiple tests will help show discrepancies, so watch for those. Poured in place slabs or even poured-in-pan can vary several inches in thickness from edge to center. Your probes will show patterned variations usually.

I document the thickness and note that the testing is done at 'X' depth, based on the GC / Owner's statement of exiting conditions. If they tell me the slab is 4" thick and it's really 14", well whose fault is it that I am only in 1.6" now?

And believe me this can and does happen!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
CONCRETE SLAB THICKNESS - MINUS - 09-02-2010, 09:48 AM
RE: CONCRETE SLAB THICKNESS - Ernesto - 09-03-2010, 08:13 AM
RE: CONCRETE SLAB THICKNESS - CC Solutions - 09-20-2010, 02:25 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,326 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 31,195 Views
Last Post by eaadams
05-19-2014, 10:55 AM
4 Replies 9,851 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 47,485 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
9 Replies 41,589 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 105,930 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 15,349 Views
Last Post by eaadams
01-30-2013, 04:43 PM
1 Replies 7,734 Views
Last Post by Rubensgt40
01-24-2013, 07:03 PM
32 Replies 96,268 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 6,151 Views
Last Post by eaadams
03-23-2012, 09:40 AM

Users browsing this thread:
1 Guest(s)