How do you guys verify the thickness of the slab? Do you core drill are look at original specs or take a an owners word?
Thanks

09-03-2010, 08:13 AM #2
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
If it's post tension I will NOT drill through the slab Big Grin New site, there's plenty of places to check or plans or pull out the shovel. I never take anyones word for anything.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

09-20-2010, 02:25 PM #3
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Well, I guess I just ask! I check the prints, look for cored holes, cut-outs at HVAC shafts, whatever, but I need to rely on the owner or General's knowledge of how thick the slab is.

That said, there is always risk that the slab isn't what they think it is! Multiple tests will help show discrepancies, so watch for those. Poured in place slabs or even poured-in-pan can vary several inches in thickness from edge to center. Your probes will show patterned variations usually.

I document the thickness and note that the testing is done at 'X' depth, based on the GC / Owner's statement of exiting conditions. If they tell me the slab is 4" thick and it's really 14", well whose fault is it that I am only in 1.6" now?

And believe me this can and does happen!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,348 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 31,278 Views
Last Post by eaadams
05-19-2014, 10:55 AM
4 Replies 9,871 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 47,573 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
9 Replies 41,639 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 106,125 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 15,381 Views
Last Post by eaadams
01-30-2013, 04:43 PM
1 Replies 7,744 Views
Last Post by Rubensgt40
01-24-2013, 07:03 PM
32 Replies 96,378 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 6,154 Views
Last Post by eaadams
03-23-2012, 09:40 AM

Users browsing this thread:
1 Guest(s)