I always wanted to run a cacl test over 6mil but never had the time. Smile

But ....I would like to do cacl and insitu tests on an open slab, then cover with 6mil and then perform the tests over after a week or so. Some cacl tests on top of the 6mil and then a cut out area for some more cacl tests that were all sealed up tight to the 6mil.

Perhaps this is the missing link to matching up cacl tests to rh testing. And as far as I know no one has ever done this before. The tests were compared to each other on an open slab, yes or no?

The cacl tests on top of the 6 mil would be just for giggles of course.

Anyone out there want to donate some testing kits and Rapid RH probes for my unscientific experiment?Cool








Messages In This Thread
CaCl vs Insitu Yet Again - Ernesto - 08-30-2010, 12:46 PM
RE: CaCl vs Insitu Yet Again - eaadams - 08-30-2010, 11:21 PM
RE: CaCl vs Insitu Yet Again - Ernesto - 08-31-2010, 07:05 AM
RE: CaCl vs Insitu Yet Again - eaadams - 08-31-2010, 11:14 AM
RE: CaCl vs Insitu Yet Again - Ernesto - 08-31-2010, 02:18 PM
RE: CaCl vs Insitu Yet Again - eaadams - 08-31-2010, 02:36 PM
RE: CaCl vs Insitu Yet Again - Ernesto - 08-31-2010, 04:09 PM
RE: CaCl vs Insitu Yet Again - CC Solutions - 09-20-2010, 02:40 PM
RE: CaCl vs Insitu Yet Again - eaadams - 09-20-2010, 02:48 PM
RE: CaCl vs Insitu Yet Again - CC Solutions - 09-20-2010, 03:06 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
20 Replies 69,277 Views
Last Post by CC Solutions
09-20-2010, 02:42 PM
2 Replies 13,177 Views
Last Post by CC Solutions
12-17-2009, 11:53 AM

Users browsing this thread:
1 Guest(s)