02-14-2011, 11:22 PM #21
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Sounds to me like you used a good adhesive like mapei's new high moisture products for engineered wood. Or it was a floating click together like a tekno. All sort of options are out there

02-15-2011, 07:57 AM #22
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(02-14-2011, 11:22 PM)eaadams Wrote:  Sounds to me like you used a good adhesive like mapei's new high moisture products for engineered wood. Or it was a floating click together like a tekno. All sort of options are out there

No, I do not glue down click systems. I used Bostik Best and thats all. I just had a feeling and the slab was full of spiderweb cracks in the surface so I figured the readings were artificially high due to the cracks.I was patching and you could virtually see the water get sucked out of the patch.

And it just looked dry.....OOOOOOOOH lolTongue


Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

02-15-2011, 10:22 AM #23
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Yes there are good adhesives out there. However, please don't think they will hide cracks. Moisture is one thing, expansion/contraction/cracks etc... is an entirely other issue that has often been the 'whipping' boy of moisture.

Cracks and slab construction type issues are interesting because now that we do have good high rH adhesives to use (almost as good as old Asbestos laden products) it will take time & education but I'm done getting sued for 'moisture' floor failures when they are really just bad 'crete. Now the concrete contractor is going to get sued (finally!) for his poor workmanship.

02-15-2011, 11:43 AM #24
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
(02-15-2011, 10:22 AM)eaadams Wrote:  Yes there are good adhesives out there. However, please don't think they will hide cracks. Moisture is one thing, expansion/contraction/cracks etc... is an entirely other issue that has often been the 'whipping' boy of moisture.

Cracks and slab construction type issues are interesting because now that we do have good high rH adhesives to use (almost as good as old Asbestos laden products) it will take time & education but I'm done getting sued for 'moisture' floor failures when they are really just bad 'crete. Now the concrete contractor is going to get sued (finally!) for his poor workmanship.

Well these were really ...lets say fractures? No? Ever see a slab with spider webed fractures or cracks? I skim coated the slab with Ardex SF. And I always patch larger cracks even when using MVP4 which they claim can bridge 1/8 inch cracks. But I've seen lots of MVP4 go down those cracks.

About those concrete contractors.....I doubt many have the technical back ground to know what all is in the mixture many recieve, so many admixtures these days. Thats another topic maybe Bob can address.

I have asked plenty of concrete contractors if they know what MVER's are, not one even knew the term so far.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

02-15-2011, 03:43 PM #25
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(02-15-2011, 11:43 AM)Ernesto Wrote:  I have asked plenty of concrete contractors if they know what MVER's are, not one even knew the term so far.

Are you talking about MVER's and SHAKR's??? Big Grin


JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

02-15-2011, 06:36 PM #26
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
You ea are the movers and shakers on this forum

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

02-16-2011, 09:54 AM #27
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
If I was a mover and shaker I'd get more peeps to join here.... I asked both of my friends and they haven't responded Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

02-16-2011, 05:13 PM #28
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Got an email from a Wagner website guru the other day. He checked out my website and gave me a couple tips. That was very nice of him. He must run this forum as well.

I keep calling Mr. Wagner but he keeps hanging up on me. Big Grin

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

02-18-2011, 10:11 AM #29
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
(02-16-2011, 05:13 PM)Ernesto Wrote:  I keep calling Mr. Wagner but he keeps hanging up on me. Big Grin

I don't think Ed would do that.... Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 9,588 Views
Last Post by CC Solutions
06-20-2012, 03:07 PM

Users browsing this thread:
1 Guest(s)