99% RH in concrete slab
  • 0 Vote(s) - 0 Average


09-20-2010, 03:15 PM #10
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
How about a failing vapor retarder (they don't last forever) or a violation of the vapor retarder?

Either way it's a SERIOUS heads up that all is not well in moisture land.

By the way, when will you install the other 35 probes the ASTM requires?

Just kidding! Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
99% RH in concrete slab - mwoody - 08-22-2010, 02:38 PM
RE: 99% RH in concrete slab - eaadams - 08-22-2010, 02:45 PM
RE: 99% RH in concrete slab - Ernesto - 08-22-2010, 09:42 PM
RE: 99% RH in concrete slab - mwoody - 08-23-2010, 05:54 AM
RE: 99% RH in concrete slab - eaadams - 08-23-2010, 09:17 AM
RE: 99% RH in concrete slab - mwoody - 08-27-2010, 07:24 AM
RE: 99% RH in concrete slab - eaadams - 08-27-2010, 11:33 AM
RE: 99% RH in concrete slab - Ernesto - 08-30-2010, 08:08 AM
RE: 99% RH in concrete slab - eaadams - 08-30-2010, 09:47 AM
RE: 99% RH in concrete slab - CC Solutions - 09-20-2010, 03:15 PM
RE: 99% RH in concrete slab - Floorguy - 02-03-2011, 12:55 PM
RE: 99% RH in concrete slab - eaadams - 02-03-2011, 01:53 PM
RE: 99% RH in concrete slab - Ernesto - 02-03-2011, 08:12 PM
RE: 99% RH in concrete slab - CC Solutions - 02-06-2011, 11:31 AM
RE: 99% RH in concrete slab - eaadams - 02-06-2011, 05:49 PM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 09:37 AM
RE: 99% RH in concrete slab - mwoody - 02-07-2011, 11:02 AM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 11:07 AM
RE: 99% RH in concrete slab - Ernesto - 02-14-2011, 08:37 PM
RE: 99% RH in concrete slab - CC Solutions - 02-14-2011, 09:06 PM
RE: 99% RH in concrete slab - eaadams - 02-14-2011, 11:22 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 07:57 AM
RE: 99% RH in concrete slab - eaadams - 02-15-2011, 10:22 AM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 11:43 AM
RE: 99% RH in concrete slab - CC Solutions - 02-15-2011, 03:43 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 06:36 PM
RE: 99% RH in concrete slab - CC Solutions - 02-16-2011, 09:54 AM
RE: 99% RH in concrete slab - Ernesto - 02-16-2011, 05:13 PM
RE: 99% RH in concrete slab - CC Solutions - 02-18-2011, 10:11 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 9,641 Views
Last Post by CC Solutions
06-20-2012, 03:07 PM

Users browsing this thread:
1 Guest(s)