Could someone point me to the right way to measure a pre WWII slab that has no moisture membrane under it?

07-09-2010, 11:29 AM #2
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Like any other slab. However you do need to relate that the test is good for only a few days to weeks depending on weather, rain etc.

IMHO a slab with a vapor barrier under it should not be influenced as much if at all if it's done correctly.

07-09-2010, 11:47 AM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
The point is there is no vapor barier.

What environmental conditions will provide the highest reading? a low rh day or a high one?

07-09-2010, 09:43 PM #4
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Hello eaadams,
What are you looking to do with this slab? If you are just looking to test it then you should test it and report the readings at the time of the test.

If however you are looking to determine the long-term suitability of installing a moisture sensitive flooring, I suggest you refer to ACI-710 which requires a moisture barrier under every slab intended to receive flooring. And all manufacturers will follow ACI 710.

No vapor retarder = unlimited failure potential.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-12-2010, 09:19 AM #5
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Yes we are putting a vapor sensitive floor covering down. I am awaiting instructions from the national tech manager of the product.

07-12-2010, 07:00 PM #6
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
As my little friend in Phoenix say's "seal it and forget it". Rolleyes








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 9,795 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 47,337 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
6 Replies 16,223 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
1 Replies 7,709 Views
Last Post by Rubensgt40
01-24-2013, 07:03 PM
10 Replies 27,451 Views
Last Post by eaadams
01-18-2013, 04:48 PM
23 Replies 77,113 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
16 Replies 45,428 Views
Last Post by CC Solutions
08-08-2011, 11:41 AM
2 Replies 14,774 Views
Last Post by CC Solutions
09-20-2010, 02:25 PM

Users browsing this thread:
1 Guest(s)