RH Meter Without Sleeves
  • 0 Vote(s) - 0 Average


06-19-2010, 02:11 PM #5
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
When we measure the relative humidity in a concrete slab, we want to isolate the horizon we read at the 40% depth or 20% depth depending on the slab.

No sleeve no correct depth. Ain't no way around that. The foil tape method is just sillyness. I have yet to hear any reply that has any merit.








Messages In This Thread
RH Meter Without Sleeves - Ernesto - 06-09-2010, 04:25 PM
RE: RH Meter Without Sleeves - CC Solutions - 06-09-2010, 08:55 PM
RE: RH Meter Without Sleeves - Ernesto - 06-13-2010, 07:49 AM
RE: RH Meter Without Sleeves - CC Solutions - 06-13-2010, 09:44 AM
RE: RH Meter Without Sleeves - Ernesto - 06-19-2010, 02:11 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 7,995 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
6 Replies 22,583 Views
Last Post by eaadams
02-09-2011, 10:36 AM
30 Replies 85,198 Views
Last Post by CC Solutions
12-11-2010, 06:11 PM

Users browsing this thread:
1 Guest(s)