Status: Offline Posts:606 Threads:33 Joined:Sep 2009
>>>So I am inclined to say that since the surface is drier compared to the bottom of the hole, the average RH will be lower compared to the RH at the bottom of the hole. But <<<

Exactly








Messages In This Thread
Reliability of RH Testing Using Removable Proves vs. Insitu Probes? - jigar0896 - 03-17-2010, 09:17 AM
RE: Reliability of RH Testing Using Removable Proves vs. Insitu Probes? - Ernesto - 03-17-2010, 06:34 PM
RE: Reliability of RH Testing Using Removable Proves vs. Insitu Probes? - Travis L - 03-18-2010, 10:10 AM
RE: Reliability of RH Testing Using Removable Proves vs. Insitu Probes? - CC Solutions - 03-18-2010, 06:16 PM