06-10-2014, 10:01 PM #1
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
I think I know the answer - but will run it past my favourite group of online moisture geeks and gurus to create a teachable moment.

A big commercial site, not fully closed yet: Re-readings done a few weeks after initial sensor insertions showed some readings actually higher than the first readings, by up to 3%.

2 x brand new sensors were put into an area approximately 100m2, the area was sealed off with plastic sheets and dehums run for a week. Three weeks after the first readings; one sensor read the same and one was higher by 2.5%.

The surface was highly burnished and a basic bead test didn't penetrate after 60 secs.

Also, the sensor which read higher was in a beam area, but it's unknown exactly how deep the beam is (throughout the site some are 400mm some are 600, all drying from both sides). If it's 600, then I definitely don't have 20% depth, it will be approximately 12% depth. Could this make for fluctuating readings?

Either way, I'm suspecting the burnished surface is seriously preventing the slab from drying.

Thoughts?

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Messages In This Thread
Moisture going up - Rubensgt40 - 06-10-2014, 10:01 PM
RE: Moisture going up - eaadams - 06-11-2014, 09:04 AM
RE: Moisture going up - Ernesto - 06-28-2014, 04:46 PM
RE: Moisture going up - Rubensgt40 - 07-05-2014, 03:18 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
13 Replies 28,025 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,286 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 10,024 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 15,078 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 73,565 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 17,044 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 25,413 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 49,670 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM
2 Replies 13,763 Views
Last Post by DeanC
03-07-2011, 03:47 PM

Users browsing this thread:
1 Guest(s)