Not this board Ray, the other Ray. I am certain you know of him.

I am the question man, not the answer man. What I find is amusing that after all these years in the industry I've seen ppl...so called experts jump on any bandwagon manufactures design only to find out years later that opinion was a myth, destroyed by science. Failed floors blamed on installers by the landfill full all for not. How many lives and reputations destroyed by bad science manufactures bring to the table.

The biggest ones now are engineered wood delaminating due to low rh. And elevated moisture levels alone destroy floors.

I think the new one might be high rh in a slab destroys floors.

I have seen the pictures of men pulling a piece of flooring, and immediately placing their CME on the slab and calling it "failure due to elevated moisture levels". Seen it in reports. Men with no flooring installation background at all inspecting floors they no nothing about other than a multiple page exam. Disturbing!!

The inspection industry needs a total redo, no grandfathering and run out the brokers.

G'day








Messages In This Thread
Adhesives and Moisture - Ernesto - 02-03-2010, 01:41 PM
RE: Adhesives and Moisture - CC Solutions - 02-03-2010, 03:53 PM
RE: Adhesives and Moisture - Ernesto - 02-05-2010, 08:12 AM
RE: Adhesives and Moisture - CC Solutions - 02-05-2010, 11:56 AM
RE: Adhesives and Moisture - Ernesto - 02-17-2010, 03:32 PM
RE: Adhesives and Moisture - CC Solutions - 02-17-2010, 10:12 PM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 09:04 AM
RE: Adhesives and Moisture - CC Solutions - 02-18-2010, 09:34 AM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 03:19 PM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 07:13 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 08:34 AM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 11:07 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 05:31 PM
RE: Adhesives and Moisture - Ernesto - 03-08-2010, 03:11 PM
RE: Adhesives and Moisture - CC Solutions - 03-09-2010, 06:48 PM
RE: Adhesives and Moisture - Ernesto - 03-10-2010, 03:06 PM
RE: Adhesives and Moisture - CC Solutions - 03-18-2010, 06:31 PM
RE: Adhesives and Moisture - Ernesto - 03-19-2010, 06:01 PM
RE: Adhesives and Moisture - tbrown - 04-08-2010, 10:24 AM
RE: Adhesives and Moisture - CC Solutions - 04-08-2010, 08:10 PM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-29-2010, 08:38 AM
RE: Adhesives and Moisture - CC Solutions - 04-30-2010, 09:03 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-30-2010, 09:33 AM
RE: Adhesives and Moisture - CC Solutions - 05-01-2010, 09:40 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 05-01-2010, 10:37 AM
RE: Adhesives and Moisture - CC Solutions - 05-02-2010, 08:18 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,936 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 37,242 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 9,159 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 12,043 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 17,847 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 84,136 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 19,686 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 29,633 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 57,214 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM

Users browsing this thread:
2 Guest(s)