02-03-2010, 01:41 PM #1
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Food for thought:

A little tidbit I found in some lit:

302.2R-18 ACI COMMITTEE REPORT

"shown that the adhesive strength decreases with an increase
in the concrete’s MVER. When these tests were conducted,
however, there were no criteria for acceptable bond strength,
and scatter in the test results did not indicate a clear dividing line
between acceptable and nonacceptable adhesive bond strength.
A report on recent testing that attempted to correlate moisture
in the concrete with floor covering performance concluded
that: “The evidence presented suggests that there is no
relationship between the relative humidity of a concrete base
or screed and adhesion of resilient floor coverings” (The
Concrete Society 2004).
While moisture criteria are often used, the relationship
between these criteria and floor covering performance is not
well understood."








Messages In This Thread
Adhesives and Moisture - Ernesto - 02-03-2010, 01:41 PM
RE: Adhesives and Moisture - CC Solutions - 02-03-2010, 03:53 PM
RE: Adhesives and Moisture - Ernesto - 02-05-2010, 08:12 AM
RE: Adhesives and Moisture - CC Solutions - 02-05-2010, 11:56 AM
RE: Adhesives and Moisture - Ernesto - 02-17-2010, 03:32 PM
RE: Adhesives and Moisture - CC Solutions - 02-17-2010, 10:12 PM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 09:04 AM
RE: Adhesives and Moisture - CC Solutions - 02-18-2010, 09:34 AM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 03:19 PM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 07:13 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 08:34 AM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 11:07 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 05:31 PM
RE: Adhesives and Moisture - Ernesto - 03-08-2010, 03:11 PM
RE: Adhesives and Moisture - CC Solutions - 03-09-2010, 06:48 PM
RE: Adhesives and Moisture - Ernesto - 03-10-2010, 03:06 PM
RE: Adhesives and Moisture - CC Solutions - 03-18-2010, 06:31 PM
RE: Adhesives and Moisture - Ernesto - 03-19-2010, 06:01 PM
RE: Adhesives and Moisture - tbrown - 04-08-2010, 10:24 AM
RE: Adhesives and Moisture - CC Solutions - 04-08-2010, 08:10 PM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-29-2010, 08:38 AM
RE: Adhesives and Moisture - CC Solutions - 04-30-2010, 09:03 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 04-30-2010, 09:33 AM
RE: Adhesives and Moisture - CC Solutions - 05-01-2010, 09:40 AM
RE: Adhesives and Moisture - Ken Larsen CR WLS - 05-01-2010, 10:37 AM
RE: Adhesives and Moisture - CC Solutions - 05-02-2010, 08:18 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,698 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 36,229 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 8,989 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 11,840 Views
Last Post by eaadams
09-27-2013, 10:26 AM
4 Replies 17,595 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 83,186 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 19,438 Views
Last Post by Ernesto
08-14-2011, 08:43 PM
8 Replies 29,233 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM
17 Replies 56,438 Views
Last Post by CC Solutions
04-01-2011, 09:02 PM

Users browsing this thread:
1 Guest(s)