Status: Offline Posts:1 Threads:1 Joined:Jan 2010
Here is my situation: Tested the conc with an RH level of 90%, using Bamboo floor covering that requires a moisture barrier. After installing the moisture barrier how do I determine if the moisture levels have reduced to the acceptable levels to install the bamboo? Do I use a CaCl test since I am now just concerned with the surface reading?
Thanks.

01-21-2010, 02:50 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
I think the two preferred methods will be the CaCl test ASTM F1869 and the RH Hood test ASTM F2420.

Personally I would use the CaCl test because that is probably what the flooring manufacturer is looking for. In this case the MVER will not vary much because of the mitigation system in place.

This test should be conducted directly on the moisture barrier, not over any patch material.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

08-30-2010, 09:59 AM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
(01-21-2010, 02:30 PM)DShenk Wrote:  the moisture barrier

Is it a moisture barrier (VAP, Planiseal, MC) or is it a vapor membrane (visquene 6mil from Home Despot) or is a low perm vapor barrier (Stego, Reef or equal) ?

08-30-2010, 12:42 PM #4
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Is it gluedown? Bamboo over a slab reading 90% Thats one I would not feel bad about walking away from.








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,496 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 27,959 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,269 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 10,007 Views
Last Post by eaadams
09-27-2013, 10:26 AM
6 Replies 15,260 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 25,989 Views
Last Post by eaadams
01-18-2013, 04:48 PM
4 Replies 15,051 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 73,452 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 17,012 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)