Here is my situation: Tested the conc with an RH level of 90%, using Bamboo floor covering that requires a moisture barrier. After installing the moisture barrier how do I determine if the moisture levels have reduced to the acceptable levels to install the bamboo? Do I use a CaCl test since I am now just concerned with the surface reading?
Thanks.








Messages In This Thread
How to test RH levels after moisture barrier is used - DShenk - 01-21-2010, 02:30 PM
RE: How to test RH levels after moisture barrier is used - CC Solutions - 01-21-2010, 02:50 PM
RE: How to test RH levels after moisture barrier is used - eaadams - 08-30-2010, 09:59 AM
RE: How to test RH levels after moisture barrier is used - Ernesto - 08-30-2010, 12:42 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 10,934 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
13 Replies 37,242 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 9,159 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
2 Replies 12,043 Views
Last Post by eaadams
09-27-2013, 10:26 AM
6 Replies 18,411 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 30,708 Views
Last Post by eaadams
01-18-2013, 04:48 PM
4 Replies 17,847 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
23 Replies 84,136 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 19,686 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)