Status: Offline Posts:600 Threads:88 Joined:Jul 2010
I got a kick out of "Worse yet, the expansion joint between the slabs had no backer rod or sealant."

I had this happen on a job. No sealant at all. We pointed it out, they fixed it. Then they sued the contractor for a new floor. Made me sick

Oh yea and how'd I find it? I followed the ant trail. Ants always find a way








Messages In This Thread
article on testing - eaadams - 07-26-2013, 12:51 PM
RE: article on testing - CCR - 07-26-2013, 04:23 PM
RE: article on testing - eaadams - 07-26-2013, 05:51 PM
RE: article on testing - CC Solutions - 09-01-2013, 09:10 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 7,874 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 10,748 Views
Last Post by eaadams
06-28-2013, 10:26 AM
27 Replies 51,448 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 42,818 Views
Last Post by CCR
03-21-2013, 05:05 PM
1 Replies 9,739 Views
Last Post by CC Solutions
10-13-2012, 08:45 PM
23 Replies 63,142 Views
Last Post by CC Solutions
07-26-2012, 06:19 AM
6 Replies 16,420 Views
Last Post by CCR
07-12-2012, 01:44 PM

Users browsing this thread:
1 Guest(s)