I was contacted by a potential client with ongoing substrate problems with a premium sheet vinyl, as well as resinous floor. The pictures provided showed clear evidence there are issues. That in itself is not as strange as my discovery on both manufacturer's websites...neither had ANY mention I could find for moisture testing...ASTM or otherwise!! Nowhere... not even in their installation instructions. Not sure if I'll get the testing assignment, but I'm dying to learn more.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

06-27-2013, 12:54 PM #2
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
If they mention ASTM F710 then there is an assumption 3# or 75%

06-28-2013, 04:31 AM #3
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
You are absolutely correct. I kept digging for the guidelines for one of the manufacturers, and only by Googling different words was I able to FINALLY find the manufacturer's "general" testing guidelines. No testing guidelines were found for the particular line of floor covering. While I am glad I found something, I question why the information was so well hidden since it was not within the installation guidelines found within their corporate and product website. Huh

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

06-28-2013, 10:26 AM #4
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
My bet, the moisture requirements are on the pail of adhesive & if you are dealing with one of the many 'distributors' who pawn themselves off as manufacturers, they change adhesives out at a whim.








Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 14,290 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 15,673 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
27 Replies 68,757 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 56,463 Views
Last Post by CCR
03-21-2013, 05:05 PM
23 Replies 79,634 Views
Last Post by CC Solutions
07-26-2012, 06:19 AM
6 Replies 21,059 Views
Last Post by CCR
07-12-2012, 01:44 PM
1 Replies 10,032 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)