Amazing Concrete Moisture Solution!
  • 0 Vote(s) - 0 Average


08-30-2013, 12:05 PM #19
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Well, this project came to a successful end so it seems. After many back and forth discussions and system evaluations, someone came up with a prep and product installation system that addressed the issue and is fully warranted. Everyone is happy and the job can finally get completed...except for the overall final cost, which the GC has to eat. Doubt seriously if the manufacturer of the original system will ever see a job from this GC ever again. Had they stuck with a proven system instead of trying to cut corners, all the delays and expense would have been avoided...expensive lesson learned.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Amazing Concrete Moisture Solution! - CCR - 05-30-2013, 05:33 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 09:33 AM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 09:59 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 05-31-2013, 02:39 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 02:52 PM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 05-31-2013, 03:11 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 03:20 PM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 05:08 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 05:35 PM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 05:44 PM
RE: Amazing Concrete Moisture Solution! - jim decker - 06-01-2013, 01:17 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-07-2013, 07:58 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:09 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:09 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:10 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:35 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:38 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:49 AM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 12:05 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-30-2013, 12:11 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 01:06 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-30-2013, 01:08 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 01:09 PM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 09-01-2013, 07:37 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 02-26-2014, 09:23 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 02-26-2014, 03:20 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
9 Replies 28,052 Views
Last Post by CC Solutions
12-26-2012, 01:02 PM
6 Replies 24,531 Views
Last Post by CC Solutions
03-27-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)