hmmmmm

That is a very good question. However F-710 doesn't have space there. Granted, my copy is from 2005, but I read it just to says that "the flooring or adhesive manufacturer or both shall be consulted" X1.3.2.

So... I guess it could certainly conform to F-710. Since F-710 refuses to actually say 'hell no'.


I have always used ASTM C309 as a barrier to such products. But if they now claim C309 conformity that changes the game. I know some of the larger concrete mitigation corps use C309 as their safety language also.








Messages In This Thread
Amazing Concrete Moisture Solution! - CCR - 05-30-2013, 05:33 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 09:33 AM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 09:59 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 05-31-2013, 02:39 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 02:52 PM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 05-31-2013, 03:11 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 03:20 PM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 05:08 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 05:35 PM
RE: Amazing Concrete Moisture Solution! - CCR - 05-31-2013, 05:44 PM
RE: Amazing Concrete Moisture Solution! - jim decker - 06-01-2013, 01:17 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-07-2013, 07:58 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:09 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:09 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:10 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:35 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-07-2013, 08:38 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 08-07-2013, 08:49 AM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 12:05 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-30-2013, 12:11 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 01:06 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 08-30-2013, 01:08 PM
RE: Amazing Concrete Moisture Solution! - CCR - 08-30-2013, 01:09 PM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 09-01-2013, 07:37 AM
RE: Amazing Concrete Moisture Solution! - eaadams - 02-26-2014, 09:23 AM
RE: Amazing Concrete Moisture Solution! - CC Solutions - 02-26-2014, 03:20 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
9 Replies 29,778 Views
Last Post by CC Solutions
12-26-2012, 01:02 PM
6 Replies 25,882 Views
Last Post by CC Solutions
03-27-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)