A byproduct of burning hydrocarbon fuels is moisture, so an improperly vented heating system can add moisture to the slab. However if fresh air is used for combustion this is usually not the case.

I tell people to begin testing slabs as soon as they can! I have installed RH probes in slabs and sealed the top with duct tape to keep water out of the probe when windows were still missing.

ATSM 2170 does have parameters to follow before RH tests are to be accepted as 'gospel' but the information gathered from early testing still has great value. Trending a slab's moisture content can help identify problems long before they become emergencies.

I'd rather tell a general that he needs to shot blast and bring in a dehumidifier system 3 months before he needs to put floor coverings down, than try to tell him that a week before he needs to start.....

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
When to Test - CFI - 11-22-2009, 11:36 AM
RE: When to Test - Ben - 11-24-2009, 12:23 PM
RE: When to Test - CC Solutions - 12-16-2009, 11:45 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 16,232 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 27,470 Views
Last Post by eaadams
01-18-2013, 04:48 PM
16 Replies 45,451 Views
Last Post by CC Solutions
08-08-2011, 11:41 AM
3 Replies 15,586 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 18,889 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 11,843 Views
Last Post by eaadams
07-09-2010, 09:45 AM
14 Replies 48,454 Views
Last Post by CC Solutions
01-15-2010, 09:36 PM
3 Replies 16,335 Views
Last Post by rthompson
11-04-2008, 10:03 AM

Users browsing this thread:
1 Guest(s)