Everyone should be reading the last two issues of Concrete Construction. Lee from IFTI did an article on CC testing. This month they had some others do a kinda softball counter argument. I'm QUITE surprised there wasn't a more significant article on RH. But perhaps that is coming with the silicate article they better produce after this year's ... bitchfest ... online after the WOC lunch discussion.

I personally use IFTI some times. However, I have discovered some of their testers trying to side sell work on these projects. Not appreciated since I'm the one that sent em there. And then I put a note in the database and said bye bye to that region for IFTI testing.








Messages In This Thread
JD's ref: RH and MVER conversion explanation - jim decker - 03-23-2013, 09:39 AM
RE: JD's ref: RH and MVER conversion explanation - CCR - 03-23-2013, 04:35 PM
RE: JD's ref: RH and MVER conversion explanation - CC Solutions - 03-25-2013, 06:26 AM
RE: JD's ref: RH and MVER conversion explanation - eaadams - 04-29-2013, 04:14 PM
RE: JD's ref: RH and MVER conversion explanation - CC Solutions - 04-29-2013, 06:53 PM
RE: JD's ref: RH and MVER conversion explanation - eaadams - 04-30-2013, 09:05 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 11,226 Views
Last Post by jim decker
07-13-2015, 02:51 PM

Users browsing this thread:
1 Guest(s)