There are a host of problems with blotter layers as they let moisture freely travel under the slab.

Installed perfectly they would work well but cause the concrete to dry more slowly.

But they are never installed perfectly. A puncture in the vapor retarder under a blotter layer will allow a huge amount of water into the blotter layer, whereas a hole in a blotter layer directly against the concrete will be nearly insignificant.

As far as RH testing goes, you need to reference the conditions assumed and indicate the requirements set forth by the flooring manufacturers and ASTM F-710. If the moisture levels change due to improper construction detail or workmanship error, you can hardly be held liable.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
insuti testing - jim decker - 03-14-2013, 02:09 PM
RE: insuti testing - CCR - 03-16-2013, 04:41 PM
RE: insuti testing - jim decker - 03-17-2013, 07:49 PM
RE: insuti testing - CC Solutions - 03-19-2013, 06:41 AM
RE: insuti testing - jim decker - 03-19-2013, 09:35 AM
RE: insuti testing - CC Solutions - 03-19-2013, 08:38 PM
RE: insuti testing - jim decker - 03-20-2013, 07:42 AM
RE: insuti testing - CC Solutions - 03-21-2013, 11:50 AM
RE: insuti testing - CCR - 03-21-2013, 05:08 PM
RE: insuti testing - jim decker - 03-22-2013, 08:45 AM
RE: insuti testing - eaadams - 04-29-2013, 04:27 PM
RE: insuti testing - CC Solutions - 04-29-2013, 07:01 PM
RE: insuti testing - eaadams - 04-30-2013, 09:15 AM
RE: insuti testing - CC Solutions - 05-01-2013, 05:57 AM
RE: insuti testing - CCR - 05-01-2013, 06:16 AM
RE: insuti testing - CC Solutions - 05-01-2013, 06:24 AM
RE: insuti testing - rapidrhrep - 05-01-2013, 10:15 AM
RE: insuti testing - CCR - 05-02-2013, 03:42 AM
RE: insuti testing - CC Solutions - 05-02-2013, 05:53 AM
RE: insuti testing - CCR - 05-02-2013, 06:33 AM
RE: insuti testing - eaadams - 05-02-2013, 08:05 AM
RE: insuti testing - CC Solutions - 05-02-2013, 08:45 AM
RE: insuti testing - eaadams - 05-02-2013, 08:59 AM
RE: insuti testing - CC Solutions - 05-02-2013, 09:02 AM
RE: insuti testing - eaadams - 05-02-2013, 10:21 AM
RE: insuti testing - CC Solutions - 05-02-2013, 11:25 AM
RE: insuti testing - eaadams - 05-02-2013, 11:30 AM
RE: insuti testing - jim decker - 05-02-2013, 12:31 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 9,055 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 12,683 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
3 Replies 11,550 Views
Last Post by eaadams
06-28-2013, 10:26 AM
23 Replies 45,519 Views
Last Post by CCR
03-21-2013, 05:05 PM
23 Replies 66,415 Views
Last Post by CC Solutions
07-26-2012, 06:19 AM
6 Replies 17,240 Views
Last Post by CCR
07-12-2012, 01:44 PM
1 Replies 8,672 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)