exposed concrete concerns
  • 0 Vote(s) - 0 Average


11-21-2009, 08:20 PM #1
insptrMarkus Newbie *
Status: Offline Posts:1 Threads:1 Joined:Nov 2009
Hi guys, this is my first post to this forum. I found this forum while searching info for an inspection. I'm a Building Inspector that does a lot of 'adverse conditions' inspections. This one is a bit out of my normal routine.
Currently I'm trying to assist a client with a problem as follows ...
New construction concrete mid-rise, occupancy started spring of this year. Client has been living in a 2 bed Condo for about 6 months and feels the place is making them sick. Unit has about 1300+ sqft. of exposed concrete on the walls and ceilings.
I took various moisture/RH readings.
Concrete surface 30-45%
1/8"-1/4" subsurface 50-75%
1" subsurface 80-99.9%
ambient RH 17-22%
At first I thought this might be an issue of emissions but based on the low ambient RH, I'm wondering if all the concrete isn't sucking the place dry.
Client states walls darken when it rains outside and portions of the floor blister up. Wood laminate floor over vapor barrier.
I've done other inspection work for this client and have made it clear that this isn't my field of expertise. I'm looking for information and ideas on what could be going on here so that I can point the client in the right direction.
I grew up in the trades on jobsites, so I'm pretty hearty and not the sensitive type. I started getting congested after an hour in the place.
Any thoughts or references for things to read are greatly appreciated.
Thanks Markus

chikiwighi Show this Post
01-10-2010, 10:55 PM #2
chikiwighi Unregistered
 
Hi,
But can you please tell me the more information.

01-11-2010, 12:51 PM #3
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
There's no waterproofing on the exterior of the concrete? Did you look behind things such as pictures, baseboards, switch plates etc? It's easy to have a mold test done, but much quicker to look for it first.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

01-12-2010, 09:49 AM #4
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Hows the ventilation system performing? Anyone check that?

Are the units below and above him being lived in?








Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 15,365 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 40,406 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 46,681 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 122,035 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 18,220 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 109,854 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 7,046 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 87,696 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
37 Replies 128,581 Views
Last Post by CC Solutions
09-20-2011, 10:07 AM
12 Replies 49,241 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM

Users browsing this thread:
1 Guest(s)