#Login Register
slab warmer than air
  • 0 Vote(s) - 0 Average


01-24-2013, 05:50 PM #1
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Here is a first. Slab is warmer than the air. (it has been colder than average in California) RH results should be lower right?

2" slab on Bitumin layer on 6" slab on an old cemetery (so they don't want to remove the slab for fear of the un-dead! har har har)

01-24-2013, 07:03 PM #2
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
Well, yeah, all things being equal the warmer air inside the slab would mean a lower %.

But if there's zombies involved, all things are not equal.

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 13,650 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 58,489 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
23 Replies 93,208 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
2 Replies 17,217 Views
Last Post by CC Solutions
09-20-2010, 02:25 PM
5 Replies 23,027 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 15,437 Views
Last Post by RCConcrete Consulting
09-21-2009, 05:17 PM
1 Replies 14,795 Views
Last Post by EWagner
07-09-2009, 01:46 PM

Users browsing this thread:
1 Guest(s)