01-17-2013, 05:13 AM #9
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
You're right about the extra trips for sure. I just charge for the extra mobilization and tell them that's the ASTM testing standard. If they don't like it, they can call somebody else and waste time and money.

As far as RH for epoxy, I'm waiting on word to proceed with RH testing at another epoxy job, but this one's failing. Turns out someone did CaCl, but not sure if it was done per F1869. More on that one later if I get it.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Cal Chlor Test - CCR - 01-13-2013, 11:00 AM
RE: Cal Chlor Test - Ernesto - 01-15-2013, 09:16 AM
RE: Cal Chlor Test - CCR - 01-15-2013, 12:20 PM
RE: Cal Chlor Test - Ernesto - 01-15-2013, 04:33 PM
RE: Cal Chlor Test - CCR - 01-15-2013, 04:56 PM
RE: Cal Chlor Test - Ernesto - 01-16-2013, 08:00 AM
RE: Cal Chlor Test - CCR - 01-16-2013, 05:20 PM
RE: Cal Chlor Test - Ernesto - 01-16-2013, 07:52 PM
RE: Cal Chlor Test - CCR - 01-17-2013, 05:13 AM
RE: Cal Chlor Test - Rubensgt40 - 01-17-2013, 03:32 PM
RE: Cal Chlor Test - eaadams - 01-18-2013, 04:48 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 18,407 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
16 Replies 50,720 Views
Last Post by CC Solutions
08-08-2011, 11:41 AM
3 Replies 16,640 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 20,639 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 12,859 Views
Last Post by eaadams
07-09-2010, 09:45 AM
14 Replies 52,331 Views
Last Post by CC Solutions
01-15-2010, 09:36 PM
2 Replies 13,493 Views
Last Post by CC Solutions
12-16-2009, 11:45 AM
3 Replies 17,591 Views
Last Post by rthompson
11-04-2008, 10:03 AM

Users browsing this thread:
1 Guest(s)