For the work site (GC using a bad mix, over troweling and in general making for wet concrete):
[Image: T89630-2T.jpg]

For the floor when I go to inspect and have tester test:
[Image: pY0vntZaTaiHdptuMgGU1Gy1Sox8yz2wgetwquI1...dTG=s220-c]

For Jason at World of Concrete:
[Image: 41Hk5yODnqL._AA160_.jpg]

For the big concrete mitigation guys who make all the money and go to the beach:
[Image: 88161800?wid=300&hei=300]

11-26-2012, 06:55 PM #2
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
I like the last one. Standard footwear down here.

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


11-27-2012, 02:04 PM #3
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Nice ha ha! How bout an orange jumpsuit?

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

11-27-2012, 05:29 PM #4
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Big Grin GREAT!!! Big Grin

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

11-27-2012, 06:11 PM #5
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
Orange jumpsuit is a great idea. That way, everyone will think we're in a religious cult. Like this...

http://youtu.be/CoCEc5B1M8Y

At least we'll have the place to ourselves and no other trades stepping on the probes!

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


11-27-2012, 06:20 PM #6
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Will we have to shave our heads, keep a pony tail, chant and burn incense as we test? That'll scare 'em off for sure!!!!!!Cool

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com

11-27-2012, 06:27 PM #7
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
At World of Concrete last year there was a Bigfoot walking the floor for Jack Links Beef Jerkey. Perhaps Wagner should have a booth babe wearing:

[Image: TP199T_OR_02.jpg]

11-27-2012, 10:07 PM #8
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
I absolutely INSIST that Jason do his next how-to video in that orange jumpsuit.

[Image: orange%2520jason.jpg]

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


11-28-2012, 07:46 AM #9
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
LMAO ha haha

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com

12-01-2012, 09:33 AM #10
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Somebody has a lot of extra time on their hands.... Dodgy

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
10 Replies 35,298 Views
Last Post by CC Solutions
04-26-2012, 07:05 PM

Users browsing this thread:
1 Guest(s)