(09-13-2011, 03:10 PM)eaadams Wrote:  Will one reader read the same as another reader? I have only one reader.

The reading value is generated in the sensor so all readers will read the same.

I have a couple readers but I'll be darned if I know where they are. I keep leaving them at jobsites so the GC or owner can read the probes. It just makes sense because some of these jobs are 3, 4 or even 7 hours away.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Reader Longevity - Ernesto - 09-21-2009, 04:27 PM
RE: Reader Longevity - EWagner - 09-22-2009, 01:26 PM
RE: Reader Longevity - eaadams - 09-13-2011, 03:10 PM
RE: Reader Longevity - CC Solutions - 09-14-2011, 07:12 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 3,840 Views
Last Post by rapidrhrep
05-17-2016, 12:26 PM
4 Replies 17,464 Views
Last Post by CC Solutions
04-17-2012, 05:31 PM

Users browsing this thread:
1 Guest(s)