A most unfortunate flooring failure!
  • 0 Vote(s) - 0 Average


11-21-2012, 10:17 AM #23
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
George Donnelly puts the same sort of language in his reports when things are high. But no implied recommendation of product as here in California they can chop your knees off for that.

"Concrete moisture content represented in this survey continues to exceed maximum permissible levels for most floor covering.... assuming floor covering installation is imminent a topically applied sealer may be needed...."

Our other major tester refuses to put any language like that in his results. Because he doesn't want to be a flooring consultant, just a pure impartial tester.








Messages In This Thread
A most unfortunate flooring failure! - CC Solutions - 11-16-2012, 09:38 AM
RE: A most unfortunate flooring failure! - Ernesto - 11-18-2012, 09:45 AM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 11:25 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 01:36 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 01:58 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 02:34 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 04:12 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 02:44 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 03:07 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-20-2012, 03:14 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:21 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:34 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:39 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:53 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 04:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:23 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:31 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:33 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:41 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:47 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:52 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 06:58 AM
RE: A most unfortunate flooring failure! - eaadams - 11-21-2012, 10:17 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 10:56 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 11:50 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 12:57 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-21-2012, 05:50 PM
RE: A most unfortunate flooring failure! - CCR - 11-22-2012, 06:31 AM
RE: A most unfortunate flooring failure! - rapidrhrep - 11-26-2012, 02:40 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-26-2012, 04:37 PM
RE: A most unfortunate flooring failure! - eaadams - 11-26-2012, 05:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-01-2012, 09:31 AM
RE: A most unfortunate flooring failure! - eaadams - 12-01-2012, 11:09 AM
RE: A most unfortunate flooring failure! - ceflooring - 12-02-2012, 05:40 PM
RE: A most unfortunate flooring failure! - CCR - 12-02-2012, 06:26 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 10:31 AM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 01:24 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 01:30 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 01:47 PM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 02:08 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 06:42 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 06:46 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 07:18 PM
RE: A most unfortunate flooring failure! - Erica - 05-31-2013, 10:09 AM
RE: A most unfortunate flooring failure! - CCR - 06-01-2013, 04:24 AM
RE: A most unfortunate flooring failure! - jim decker - 06-01-2013, 01:12 PM
RE: A most unfortunate flooring failure! - Ernesto - 06-02-2013, 09:58 AM
RE: A most unfortunate flooring failure! - jim decker - 06-19-2013, 11:05 AM
RE: A most unfortunate flooring failure! - CCR - 06-20-2013, 04:39 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
7 Replies 20,935 Views
Last Post by Ernesto
11-02-2012, 07:44 PM
5 Replies 17,995 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)