11-20-2012, 05:23 PM #16
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Construction budget or not, the installer can protect themselves. But they have to have the nads to do it.

Taking an RH test is easy and inexpensive. Turning down the job may be the best money they ever lost. Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
A most unfortunate flooring failure! - CC Solutions - 11-16-2012, 09:38 AM
RE: A most unfortunate flooring failure! - Ernesto - 11-18-2012, 09:45 AM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 11:25 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 01:36 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 01:58 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 02:34 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 04:12 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 02:44 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 03:07 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-20-2012, 03:14 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:21 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:34 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:39 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:53 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 04:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:23 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:31 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:33 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:41 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:47 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:52 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 06:58 AM
RE: A most unfortunate flooring failure! - eaadams - 11-21-2012, 10:17 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 10:56 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 11:50 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 12:57 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-21-2012, 05:50 PM
RE: A most unfortunate flooring failure! - CCR - 11-22-2012, 06:31 AM
RE: A most unfortunate flooring failure! - rapidrhrep - 11-26-2012, 02:40 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-26-2012, 04:37 PM
RE: A most unfortunate flooring failure! - eaadams - 11-26-2012, 05:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-01-2012, 09:31 AM
RE: A most unfortunate flooring failure! - eaadams - 12-01-2012, 11:09 AM
RE: A most unfortunate flooring failure! - ceflooring - 12-02-2012, 05:40 PM
RE: A most unfortunate flooring failure! - CCR - 12-02-2012, 06:26 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 10:31 AM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 01:24 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 01:30 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 01:47 PM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 02:08 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 06:42 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 06:46 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 07:18 PM
RE: A most unfortunate flooring failure! - Erica - 05-31-2013, 10:09 AM
RE: A most unfortunate flooring failure! - CCR - 06-01-2013, 04:24 AM
RE: A most unfortunate flooring failure! - jim decker - 06-01-2013, 01:12 PM
RE: A most unfortunate flooring failure! - Ernesto - 06-02-2013, 09:58 AM
RE: A most unfortunate flooring failure! - jim decker - 06-19-2013, 11:05 AM
RE: A most unfortunate flooring failure! - CCR - 06-20-2013, 04:39 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
7 Replies 19,707 Views
Last Post by Ernesto
11-02-2012, 07:44 PM
5 Replies 17,012 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)