Thanks JD, I agree. I am not an installer either. However, I do owe my career to flooring contractors and installers. Most installers want to do good work and most do! It is unfortunate that they dwell in a highly competitive environment and its certainly not their fault that construction budgets do not allow enough money for them to protect themselves. One of our objectives is to do our part in changing the status quo and providing services that protect the installation industry as well as all party's involved.

Steve Anderson
President
Surface Testing Group








Messages In This Thread
A most unfortunate flooring failure! - CC Solutions - 11-16-2012, 09:38 AM
RE: A most unfortunate flooring failure! - Ernesto - 11-18-2012, 09:45 AM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 11:25 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 01:36 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 01:58 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 02:34 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 04:12 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 02:44 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 03:07 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-20-2012, 03:14 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:21 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:34 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:39 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:53 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 04:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:23 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:31 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:33 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:41 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:47 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:52 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 06:58 AM
RE: A most unfortunate flooring failure! - eaadams - 11-21-2012, 10:17 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 10:56 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 11:50 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 12:57 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-21-2012, 05:50 PM
RE: A most unfortunate flooring failure! - CCR - 11-22-2012, 06:31 AM
RE: A most unfortunate flooring failure! - rapidrhrep - 11-26-2012, 02:40 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-26-2012, 04:37 PM
RE: A most unfortunate flooring failure! - eaadams - 11-26-2012, 05:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-01-2012, 09:31 AM
RE: A most unfortunate flooring failure! - eaadams - 12-01-2012, 11:09 AM
RE: A most unfortunate flooring failure! - ceflooring - 12-02-2012, 05:40 PM
RE: A most unfortunate flooring failure! - CCR - 12-02-2012, 06:26 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 10:31 AM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 01:24 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 01:30 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 01:47 PM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 02:08 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 06:42 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 06:46 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 07:18 PM
RE: A most unfortunate flooring failure! - Erica - 05-31-2013, 10:09 AM
RE: A most unfortunate flooring failure! - CCR - 06-01-2013, 04:24 AM
RE: A most unfortunate flooring failure! - jim decker - 06-01-2013, 01:12 PM
RE: A most unfortunate flooring failure! - Ernesto - 06-02-2013, 09:58 AM
RE: A most unfortunate flooring failure! - jim decker - 06-19-2013, 11:05 AM
RE: A most unfortunate flooring failure! - CCR - 06-20-2013, 04:39 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
7 Replies 22,608 Views
Last Post by Ernesto
11-02-2012, 07:44 PM
5 Replies 19,435 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)