A most unfortunate flooring failure!
  • 0 Vote(s) - 0 Average


11-18-2012, 09:45 AM #2
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Yes, I just did a similar moisture testing gig for a firm who put an epoxy coating on a drive outside a hotel driveway. But, no effloressence just some blistering. I felt it was improper prep instead of a moisture issue even though I got high readings.

The old epoxy had not been taken off and it was pulling as well. Multiple layering of the epoxy by the maintenance staff before this contractor got there.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
A most unfortunate flooring failure! - CC Solutions - 11-16-2012, 09:38 AM
RE: A most unfortunate flooring failure! - Ernesto - 11-18-2012, 09:45 AM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 11:25 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 01:36 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 01:58 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-19-2012, 02:34 PM
RE: A most unfortunate flooring failure! - eaadams - 11-19-2012, 04:12 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 02:44 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 03:07 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-20-2012, 03:14 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:21 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:34 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 03:39 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 03:53 PM
RE: A most unfortunate flooring failure! - surfacesteve - 11-20-2012, 04:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:23 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:31 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:33 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:41 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-20-2012, 05:47 PM
RE: A most unfortunate flooring failure! - CCR - 11-20-2012, 05:52 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 06:58 AM
RE: A most unfortunate flooring failure! - eaadams - 11-21-2012, 10:17 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 10:56 AM
RE: A most unfortunate flooring failure! - CC Solutions - 11-21-2012, 11:50 AM
RE: A most unfortunate flooring failure! - CCR - 11-21-2012, 12:57 PM
RE: A most unfortunate flooring failure! - Rubensgt40 - 11-21-2012, 05:50 PM
RE: A most unfortunate flooring failure! - CCR - 11-22-2012, 06:31 AM
RE: A most unfortunate flooring failure! - rapidrhrep - 11-26-2012, 02:40 PM
RE: A most unfortunate flooring failure! - CC Solutions - 11-26-2012, 04:37 PM
RE: A most unfortunate flooring failure! - eaadams - 11-26-2012, 05:48 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-01-2012, 09:31 AM
RE: A most unfortunate flooring failure! - eaadams - 12-01-2012, 11:09 AM
RE: A most unfortunate flooring failure! - ceflooring - 12-02-2012, 05:40 PM
RE: A most unfortunate flooring failure! - CCR - 12-02-2012, 06:26 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 10:31 AM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 01:24 PM
RE: A most unfortunate flooring failure! - CC Solutions - 12-03-2012, 01:30 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 01:47 PM
RE: A most unfortunate flooring failure! - CCR - 12-03-2012, 02:08 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 06:42 PM
RE: A most unfortunate flooring failure! - eaadams - 12-03-2012, 06:46 PM
RE: A most unfortunate flooring failure! - Ernesto - 12-03-2012, 07:18 PM
RE: A most unfortunate flooring failure! - Erica - 05-31-2013, 10:09 AM
RE: A most unfortunate flooring failure! - CCR - 06-01-2013, 04:24 AM
RE: A most unfortunate flooring failure! - jim decker - 06-01-2013, 01:12 PM
RE: A most unfortunate flooring failure! - Ernesto - 06-02-2013, 09:58 AM
RE: A most unfortunate flooring failure! - jim decker - 06-19-2013, 11:05 AM
RE: A most unfortunate flooring failure! - CCR - 06-20-2013, 04:39 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
7 Replies 22,890 Views
Last Post by Ernesto
11-02-2012, 07:44 PM
5 Replies 19,685 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)