All:

Throw away the white tools and get the black tool. Use this tool the way I mentioned earlier; the middle step of the three step tool, is used to verify hole diameter, its a "go no-go" gauge. If it does not go down in the hole with little friction, the hole is undersized and visa versa. As far as the insertion tool pushing on the "sensor" during installation, it does, but on a very small portion. Look at how there is a small diameter change at the bottom of the tool. Also, there is ALOT of pressure taken off during installation because the tools downward pressure is spread over the top lip of the sensor barrel. The feedback I have gotten from MOST people is that if you use the new black insertion tool in the above mentioned fashion, the probes aren't any more "delicate" they just require a different method of insertion.

http://www.wagnermeters.com/video-install.php

Don't laugh to much, this is my "homemade" video. The new "professional version is due out soon.

Jason








Messages In This Thread
Bad Sensor - Ernesto - 11-07-2012, 04:36 PM
RE: Bad Sensor - rapidrhrep - 11-07-2012, 07:46 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 07:16 AM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:55 AM
RE: Bad Sensor - Rubensgt40 - 11-08-2012, 05:56 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 08:30 PM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:44 PM
RE: Bad Sensor - Ernesto - 11-09-2012, 06:33 PM
RE: Bad Sensor - Rubensgt40 - 11-10-2012, 01:11 AM
RE: Bad Sensor - Ernesto - 11-10-2012, 08:43 AM
RE: Bad Sensor - CC Solutions - 11-15-2012, 02:37 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 04:09 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 06:02 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 07:51 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 09:49 PM
RE: Bad Sensor - Ernesto - 11-16-2012, 06:51 AM
RE: Bad Sensor - Rubensgt40 - 11-21-2012, 05:35 PM
RE: Bad Sensor - CC Solutions - 11-21-2012, 08:14 PM
RE: Bad Sensor - CCR - 11-22-2012, 06:50 AM
RE: Bad Sensor - Ernesto - 11-22-2012, 09:31 AM
RE: Bad Sensor - Rubensgt40 - 11-22-2012, 06:03 PM
RE: Bad Sensor - CCR - 11-23-2012, 11:51 AM
RE: Bad Sensor - Ernesto - 11-24-2012, 09:14 AM
RE: Bad Sensor - CCR - 11-25-2012, 07:17 AM
RE: Bad Sensor - Ernesto - 11-26-2012, 09:25 AM
RE: Bad Sensor - rapidrhrep - 11-26-2012, 03:50 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 04:32 PM
RE: Bad Sensor - Rubensgt40 - 11-26-2012, 06:57 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 09:07 PM
RE: Bad Sensor - eaadams - 11-27-2012, 09:14 AM
RE: Bad Sensor - Ernesto - 11-27-2012, 02:00 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 03:33 PM
RE: Bad Sensor - CCR - 11-27-2012, 05:27 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 06:22 PM
RE: Bad Sensor - rapidrhrep - 11-28-2012, 09:58 AM
RE: Bad Sensor - Ernesto - 11-28-2012, 10:06 AM
RE: Bad Sensor - surfacesteve - 11-30-2012, 09:53 AM
RE: Bad Sensor - Ernesto - 11-30-2012, 05:09 PM
RE: Bad Sensor - eaadams - 11-30-2012, 05:33 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 08:24 AM
RE: Bad Sensor - Ernesto - 12-01-2012, 05:18 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 06:44 PM
RE: Bad Sensor - Ernesto - 12-03-2012, 06:48 PM
RE: Bad Sensor - Rubensgt40 - 12-03-2012, 06:59 PM
RE: Bad Sensor - Ernesto - 12-04-2012, 07:57 AM
RE: Bad Sensor - CC Solutions - 12-04-2012, 10:38 AM
RE: Bad Sensor - Ernesto - 12-04-2012, 08:28 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 07:23 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:00 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 08:35 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:45 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 09:54 AM
RE: Bad Sensor - CCR - 12-05-2012, 12:05 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 12:58 PM
RE: Bad Sensor - Ernesto - 12-06-2012, 06:41 PM
RE: Bad Sensor - CCR - 12-07-2012, 04:36 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 07:24 AM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:32 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 06:44 PM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:13 PM
RE: Bad Sensor - Ernesto - 12-08-2012, 08:32 AM
RE: Bad Sensor - Ernesto - 12-10-2012, 04:48 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 9,679 Views
Last Post by Ben
11-09-2009, 04:39 PM

Users browsing this thread:
1 Guest(s)