Bad Sensor
  • 0 Vote(s) - 0 Average


11-07-2012, 07:46 PM #2
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:85 Threads:3 Joined:Aug 2011
Ernesto:

You just bought a new kit with the new black instertion tool correct? How much force did you have to exert to install the sensor? Probably a stupid question but you did try to take readings a few different times correct? As Wagner always does, if there is an issue, we will rectify it. Let me know the answers and we will go from there.

Jason








Messages In This Thread
Bad Sensor - Ernesto - 11-07-2012, 04:36 PM
RE: Bad Sensor - rapidrhrep - 11-07-2012, 07:46 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 07:16 AM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:55 AM
RE: Bad Sensor - Rubensgt40 - 11-08-2012, 05:56 PM
RE: Bad Sensor - Ernesto - 11-08-2012, 08:30 PM
RE: Bad Sensor - rapidrhrep - 11-08-2012, 10:44 PM
RE: Bad Sensor - Ernesto - 11-09-2012, 06:33 PM
RE: Bad Sensor - Rubensgt40 - 11-10-2012, 01:11 AM
RE: Bad Sensor - Ernesto - 11-10-2012, 08:43 AM
RE: Bad Sensor - CC Solutions - 11-15-2012, 02:37 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 04:09 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 06:02 PM
RE: Bad Sensor - Ernesto - 11-15-2012, 07:51 PM
RE: Bad Sensor - CC Solutions - 11-15-2012, 09:49 PM
RE: Bad Sensor - Ernesto - 11-16-2012, 06:51 AM
RE: Bad Sensor - Rubensgt40 - 11-21-2012, 05:35 PM
RE: Bad Sensor - CC Solutions - 11-21-2012, 08:14 PM
RE: Bad Sensor - CCR - 11-22-2012, 06:50 AM
RE: Bad Sensor - Ernesto - 11-22-2012, 09:31 AM
RE: Bad Sensor - Rubensgt40 - 11-22-2012, 06:03 PM
RE: Bad Sensor - CCR - 11-23-2012, 11:51 AM
RE: Bad Sensor - Ernesto - 11-24-2012, 09:14 AM
RE: Bad Sensor - CCR - 11-25-2012, 07:17 AM
RE: Bad Sensor - Ernesto - 11-26-2012, 09:25 AM
RE: Bad Sensor - rapidrhrep - 11-26-2012, 03:50 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 04:32 PM
RE: Bad Sensor - Rubensgt40 - 11-26-2012, 06:57 PM
RE: Bad Sensor - CC Solutions - 11-26-2012, 09:07 PM
RE: Bad Sensor - eaadams - 11-27-2012, 09:14 AM
RE: Bad Sensor - Ernesto - 11-27-2012, 02:00 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 03:33 PM
RE: Bad Sensor - CCR - 11-27-2012, 05:27 PM
RE: Bad Sensor - Ernesto - 11-27-2012, 06:22 PM
RE: Bad Sensor - rapidrhrep - 11-28-2012, 09:58 AM
RE: Bad Sensor - Ernesto - 11-28-2012, 10:06 AM
RE: Bad Sensor - surfacesteve - 11-30-2012, 09:53 AM
RE: Bad Sensor - Ernesto - 11-30-2012, 05:09 PM
RE: Bad Sensor - eaadams - 11-30-2012, 05:33 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 08:24 AM
RE: Bad Sensor - Ernesto - 12-01-2012, 05:18 PM
RE: Bad Sensor - CC Solutions - 12-01-2012, 06:44 PM
RE: Bad Sensor - Ernesto - 12-03-2012, 06:48 PM
RE: Bad Sensor - Rubensgt40 - 12-03-2012, 06:59 PM
RE: Bad Sensor - Ernesto - 12-04-2012, 07:57 AM
RE: Bad Sensor - CC Solutions - 12-04-2012, 10:38 AM
RE: Bad Sensor - Ernesto - 12-04-2012, 08:28 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 07:23 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:00 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 08:35 AM
RE: Bad Sensor - CCR - 12-05-2012, 08:45 AM
RE: Bad Sensor - CC Solutions - 12-05-2012, 09:54 AM
RE: Bad Sensor - CCR - 12-05-2012, 12:05 PM
RE: Bad Sensor - CC Solutions - 12-05-2012, 12:58 PM
RE: Bad Sensor - Ernesto - 12-06-2012, 06:41 PM
RE: Bad Sensor - CCR - 12-07-2012, 04:36 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 07:24 AM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:32 AM
RE: Bad Sensor - Ernesto - 12-07-2012, 06:44 PM
RE: Bad Sensor - CC Solutions - 12-07-2012, 07:13 PM
RE: Bad Sensor - Ernesto - 12-08-2012, 08:32 AM
RE: Bad Sensor - Ernesto - 12-10-2012, 04:48 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 10,055 Views
Last Post by Ben
11-09-2009, 04:39 PM

Users browsing this thread:
1 Guest(s)